Its crystal structure is characterized by a three-dimensional network of ion-conducting channels, which has a high degree of ionic conductivity and can effectively facilitate the transport of lithium ions in the solid electrolyte.
IONIC CONDUCTIVITY(POWDER UNPRESSURIZED): ~8mS/cm@27℃
IONIC CONDUCTIVITY(POWDER COLD PRESSED): ~12mS/cm@27℃
ELECTRONIC CONDUCTIVITY(POWDER COLD PRESSED): <1 × 10⁻⁸ S/cm@27℃
CONDUCTIVITY ACTIVATION ENERGY (POWDER COLD PRESSED): 0.275 eV(26.6 kJ/mol) (25~85℃)
THEORETICAL DENSITY: 2g/cm³